Xenotime-(Y) (var. Nd doped) PL/Laser spectrum, 532 nm Nd:YAG laser beam, Lenz et al. 2013

Measurement details

Description PL/Laser spectrum of Xenotime-(Y) (var Syn, Nd doped)
Reference Lenz et al. 2013
Lenz C., Talla D., Ruschel K., Skoda R., Gotze J. & Nasdala L. (2013). Factors affecting the Nd(3+) (REE(3+)) luminescence of minerals. Mineral Petrol, 107, 415-428. DOI: https://doi.org/10.1007/s00710-013-0286-2
Material Xenotime-(Y) (var. Nd doped) [ YPO4:Nd ]
Specimen temperature Ambient
Technique Laser photoluminescence (PL)
Instrument Horiba LabRAM HR
Probe 532 nm Nd:YAG laser beam
Probe diameter 1.5 μm
Det. technology CCD, Si, Peltier cooled
Grating spacing 600 lines/mm
Numerical aperture 0.9
Channel count 3605
Energy range 1.302 … 1.61191 eV
Intensity range 1.31104 … 12861.1 counts
Integral 849326 counts
Lines Nd3+ 1.42174 eV (100%), 1.41514 eV (21%), 1.40708 eV (6%), 1.4004 eV (8%), 1.389 eV (5%), 1.38478 eV (7%), 1.3716 eV (4%), 1.365 eV (10%)

Composition

Nominal composition of Xenotime-(Y) (var.Nd doped) [ YPO4:Nd ].
Element Atoms At% Wt%
Y 1 16.7 48.4
P 1 16.7 16.8
O 4 66.7 34.8

Measurement spectrum

Loading...

Measurement image

Image of PL/Laser spectrum of Xenotime-(Y) (var Syn, Nd doped)