Forsterite CL/TEM measurement, 120 keV e- beam, 276K, Benstock et al. 1997
Measurement details
Reference | Benstock et al. 1997 Benstock E. J., Buseck P. R. & Steele I. M. (1997). Cathodoluminescence of meteoritic and synthetic forsterite at 296 and 77 K using TEM. American Mineralogist, 82(3-4), 310-315. DOI: https://doi.org/10.2138/am-1997-3-409 |
Material | Forsterite [ Mg2SiO4 ] |
Specimen temperature | 276K |
Technique | Cathodoluminescence (CL), using a Transmission Electron Microscope (TEM) |
Instrument | Philips 400T TEM |
Probe | 120 keV electron beam |
Probe diameter | 14 μm |
Slit width | 500 μm |
Lines | Cr3+ 721 nm, 790 nm, Mn2+ 630 nm, Unknown 410 nm |
Composition
Element | Atoms | At% | Wt% |
---|---|---|---|
Mg | 2 | 28.6 | 34.6 |
Si | 1 | 14.3 | 20 |
O | 4 | 57.1 | 45.5 |