Zircon (var. Dy doped) PL/Laser spectrum, 532 nm laser beam, Lenz et al. 2015
Measurement details
Description | PL/Laser spectrum of Zircon (var. Dy doped) |
Reference | Lenz et al. 2015 Lenz C., Nasdala L., Talla D., Hauzenberger C., Seitz R. & Kolitsch U. (2015). Laser-induced REE3+ photoluminescence of selected accessory minerals — An “advantageous artefact” in Raman spectroscopy. Chemical Geology, 415, 1-16. https://doi.org/10.1016/j.chemgeo.2015.09.001 https://www.sciencedirect.com/science/article/pii/S000925411530022X |
Material | Zircon (var. Dy doped) [ ZrSiO4:Dy ] |
Technique | Laser photoluminescence (PL) |
Instrument | Horiba LabRAM HR |
Probe | 532 nm laser beam |
Det. technology | CCD, Si, Peltier cooled |
Grating spacing | 600 lines/mm |
Numerical aperture | 0.9 |
Channel count | 9990 |
Energy range | 1.32684 … 2.97551 eV |
Intensity range | 100 (normalised intensity) |
Lines | Dy3+ 2.11947 eV (7.6%), 2.13351 eV (84.2%), 2.14017 eV (100%), 2.14777 eV (59.7%), 2.15353 eV (53.3%), 2.15854 eV (16.1%), 2.16872 eV (35.1%), 2.17421 eV (26.7%), 2.18194 eV (10.5%), 2.18677 eV (6%), 2.53705 eV (13.9%), 2.54643 eV (14.5%), 2.55142 eV (8%), 2.55789 eV (8%), 2.57044 eV (21%), 2.57701 eV (16.9%), 2.58992 eV (5.8%), 2.60165 eV (5.2%), 2.61459 eV (4.2%), 2.62056 eV (16.4%), 2.56493 eV (3.2%), 1.642 eV (5.2%), 1.8663 eV (4%), 1.8806 eV (3.2%), 1.8635 eV (3.2%), 1.8505 eV (2.9%), 1.8537 eV (2.8%), 1.8939 eV (1.4%) |
Composition
Element | Atoms | At% | Wt% |
---|---|---|---|
Zr | 1 | 16.7 | 49.8 |
Si | 1 | 16.7 | 15.3 |
O | 4 | 66.7 | 34.9 |
Measurement spectrum