Xenotime-(Y) (var. Tm doped) PL/Laser spectrum, 532 nm Nd:YAG laser beam, Lenz et al. 2013

Measurement details

Description PL/Laser spectrum of Xenotime-(Y) (var Syn, Tm doped)
Reference Lenz et al. 2013
Lenz C., Talla D., Ruschel K., Skoda R., Gotze J. & Nasdala L. (2013). Factors affecting the Nd(3+) (REE(3+)) luminescence of minerals. Mineral Petrol, 107, 415-428. DOI: https://doi.org/10.1007/s00710-013-0286-2
Material Xenotime-(Y) (var. Tm doped) [ YPO4:Tm ]
Specimen temperature Ambient
Technique Laser photoluminescence (PL)
Instrument Horiba LabRAM HR
Probe 532 nm Nd:YAG laser beam
Probe diameter 1.5 μm
Det. technology CCD, Si, Peltier cooled
Grating spacing 600 lines/mm
Numerical aperture 0.9
Channel count 10872
Energy range 1.30818 … 2.61628 eV
Intensity range -2.22974 … 28064.8 counts
Integral 1.4542×107 counts
Lines Tm3+ 1.89679 eV (97%), 1.91438 eV (81%), 1.9063 eV (43%), 1.87911 eV (23%), 1.59769 eV (74%), 1.5801 eV (43%), 1.5835 eV (30%), 1.9306 eV (21%), 1.9372 eV (17%), 2.58165 eV (100%), 1.55377 eV (26%)

Composition

Nominal composition of Xenotime-(Y) (var.Tm doped) [ YPO4:Tm ].
Element Atoms At% Wt%
Y 1 16.7 48.4
P 1 16.7 16.8
O 4 66.7 34.8

Measurement spectrum

Loading...

Measurement image

Image of PL/Laser spectrum of Xenotime-(Y) (var Syn, Tm doped)