Xenotime-(Y) (var. Sm doped) PL/Laser spectrum, 532 nm Nd:YAG laser beam, Lenz et al. 2013

Measurement details

Description PL/Laser spectrum of Xenotime-(Y) (var Syn, Sm doped)
Reference Lenz et al. 2013
Lenz C., Talla D., Ruschel K., Skoda R., Gotze J. & Nasdala L. (2013). Factors affecting the Nd(3+) (REE(3+)) luminescence of minerals. Mineral Petrol, 107, 415-428. DOI: https://doi.org/10.1007/s00710-013-0286-2
Material Xenotime-(Y) (var. Sm doped) [ YPO4:Sm ]
Specimen temperature Ambient
Technique Laser photoluminescence (PL)
Instrument Horiba LabRAM HR
Probe 532 nm Nd:YAG laser beam
Probe diameter 1.5 μm
Det. technology CCD, Si, Peltier cooled
Grating spacing 600 lines/mm
Numerical aperture 0.9
Channel count 9791
Energy range 1.30202 … 2.47983 eV
Intensity range -42.2052 … 52851.2 counts
Integral 1.7173×107 counts
Lines Sm3+ 1.92238 eV (69%), 1.9154 eV (31%), 1.9032 eV (49%), 2.2022 eV (44%), 2.06381 eV (100%), 2.0571 eV (80%), 2.0827 eV (44%), 1.7281 — 1.79003 eV (11%)

Composition

Nominal composition of Xenotime-(Y) (var.Sm doped) [ YPO4:Sm ].
Element Atoms At% Wt%
Y 1 16.7 48.4
P 1 16.7 16.8
O 4 66.7 34.8

Measurement spectrum

Loading...

Measurement image

Image of PL/Laser spectrum of Xenotime-(Y) (var Syn, Sm doped)